    济南彩钢瓦防水施工方法
    发布来源:http://www.jnjgcg.com/  2017-2-14 16:00:58 发布人:济南坚固彩钢
    用彩钢瓦的人都知道,漏水是一件很头疼的事,那怎么才能防止或降低这种情况的发生呢,下面就有答案。 如果要美观,那只有用无纺布和JS涂料贴上窟窿,或者用SBS卷材贴好后涂上同彩钢瓦一样颜色的防水涂料就可以了。硅胶时间长了经过日晒雨淋会起皮的。做防水前,窟窿部位四周一定要干净,并用砂纸打磨过,这样粘结率就牢靠了。要大于彩钢瓦窟窿一倍铺贴。实践中是完全可以一劳永逸。
    With the steel tile people know, Water Leakage is a very troublesome thing, how to prevent or reduce the occurrence of such a situation, here are the answer. If you are beautiful, that is only useful non-woven fabrics and JS coating paste hole, or waterproof coating with SBS membrane coated with good paste like color steel tile color on it. Silica gel for a long time through the sun and rain will skin. Waterproof, hole around the site must be clean and polished with sandpaper, such as firm bond rate.
    1.新彩钢瓦或者彩钢瓦表面无生锈腐蚀。工艺:无胎体基布,整体涂刷2~3遍有机硅防水涂料+板缝搭接处10cm宽的胎体基布摊铺补缝。彩钢瓦表面尚未破损,预防可能出现的生锈、延长使用寿命,降低施工成本,每平方米涂料用量不低于1公斤。在不显着提高施工成本的情况下,可至少延长彩钢瓦使用寿命5~8年。
    More than double the paving tile hole. Practice is completely possible once and for all.
    No rust corrosion of 1 new color steel tile or tile surface. Process: no carcass fabric, overall brushing 2~3 times 10cm wide spread matrix substrate organic silicon waterproof coating + lap seam paving slab. Tile surfaces have not been damaged, to prevent possible rust, prolong service life, reduce the construction cost per square metre, coating amount not less than 1 kg. In does not significantly improve the construction cost of the case, at least can prolong the service life of 5~8 steel tile.
    2.彩钢瓦表面已经出现明显的生锈腐蚀破损,或者彩钢瓦在酸碱等易腐蚀环境下使用。如果彩钢瓦表面有锈斑存在,则要先用打磨机或砂纸将表面浮锈打磨干净;如果已出现破损孔洞,则在打磨完毕,整体铺布前先用适当大小的无纺布摊铺到生锈空洞部位,作为加强处理,然后再整体摊铺胎体基布。采用此方案后,彩钢瓦的使用寿命可延长10~15年。
    2 color steel tile surface has been significantly damaged or rust corrosion, acid and other corrosive steel tile in environment. If the color steel tile surface rust, need to use the polishing machine or sand the surface rust polished clean; if you have broken holes in grinding, first with the appropriate size of the non-woven stalls shop to rust empty positions of the whole spreading, as strengthening treatment, and then the whole carcass paving fabric. Using this scheme, the steel tile service life can be prolonged to 10~15 years.
    以上两种方案均可大幅度提高彩钢瓦的使用寿命,显着降低彩钢瓦的维护费用。
    The above two methods can greatly improve the service life of the steel tile, significantly reduce the maintenance cost of color steel tile.