    岩棉复合板的安装离不开哪些流程?
    发布来源:http://www.jnjgcg.com/  2018-8-10 19:46:10 发布人:济南坚固彩钢
    首先,将岩棉复合板的表面的泥土、杂物等清理干净,对混凝土的基层进行预制或现浇。
    Firstly, the soil and sundries on the surface of the rock wool composite board are cleaned up, and the concrete base is prefabricated or cast in place.
    其次,是岩棉复合保温层铺设,主要分为:
    Secondly, the rock wool composite insulation layer is mainly divided into:
    1、铺设前应先将其接触面进行清洗,应找平拉线进行干铺岩棉复合板,板块之间铺平、紧密,若是分层铺设的板块,应将其上下两层错开,找同类材料的碎屑将板块之间的缝隙填密紧实,同时表面应与相邻两板的高度一致。
    1. Before laying, the contact surface should be cleaned, and the drawing line should be leveled for dry laying of rock wool composite plate. If the plate is layered, the upper and lower layers should be staggered, and the cracks between the plates should be tightened by looking for the debris of the same material, and the surface should be consistent with the height of the adjacent two plates.

    2、在做砂浆找平层分格缝排气道处留设,当板状保温层如需留设排汽槽时,不得有遗漏现象出现。

    济南复合板厂

    2. Leave the exhaust duct at the slotted joint of the mortar leveling layer. When the plate insulation layer needs to leave the exhaust slot, there must be no omission.
    3、岩棉复合板保温层已铺完当在上面进行行走或用胶轮车运输材料时,应垫上脚手板进行保护。
    3. The insulation layer of rock wool composite board has been laid. When walking on it or transporting materials by rubber wheel truck, the scaffold board should be padded for protection.
    4、当复合板出现缺棱掉角的现象时,可用同类材料的碎块进行嵌补。
    4. When the composite plate appears the phenomenon of missing edge and missing angle, the same kind of material can be used for patching.
    更后,是保护层的安装:
    Finally, the installation of the protective layer:
    1、上人屋面:
    1. Upper roof:
    A、当上人屋面采用的是混凝土块做面层时,板缝之间有间隙时应用砂浆勾缝处理,并且采用水泥砂浆座浆铺平。
    A. When the upper roof is made of concrete blocks, when there are gaps between the slab joints, the use of mortar seam treatment, and the use of cement mortar base mortar paving.
    B、若面层采用的是40-50mm厚钢筋细石混凝土时,应进行分格缝的节点处理按照钢性防水层的设计要求。
    B. If the surface layer is 40-50mm thick reinforced fine stone concrete, should be divided into grid joint treatment according to the design requirements of steel waterproof layer.
    2、不上人屋面:
    2. No roof.
    A、若采用的是非功能性屋面作为屋面时,可以对其进行处理采用平铺预制混凝土板的方式。预制板的厚度应小于30mm,并具有一定的强度。
    A. If the non-functional roof is used as the roof, it can be treated by the way of flat precast concrete slab. The thickness of precast slab should be less than 30mm and has a certain intensity.
    B、当选用的是卵石或者是砂砾作为保护层时,直径应在20-60mm范围之内,并且要注意雨水口保持畅通。
    B. When using pebble or gravel as protective layer, the diameter should be in the range of 20-60 mm, and should pay attention to keeping the nozzle open.